Small punch creep test of service-exposed SUS 316 HTB superheater tubes of fossil boilers

Maribel L. Saucedo-Muñoz, Shin Ichi Komazci, Toru Takahashi, Toshiyuki Hashida, Tetsuo Shoji, Victor M. Lopez-Hirata

Producción científica: Capítulo del libro/informe/acta de congresoContribución a la conferenciarevisión exhaustiva

Resumen

The creep properties were evaluated in a SUS 316 HTB austenitic stainless steel by using the small-punch creep test. The applied loads were 234, 286. 338, 408 and 478 N at 650 °C, and 199 and 234 N at 700 °C. The creep curves were similar to those obtained from a conventional uniaxial creep test. That is, they exhibited clearly the three creep stages. The width of secondary creep stage and rupture time tr decreased with the increase in testing load level. The creep rupture strength for the service-exposed material was lower than that of the as-received material at high testing loads. While, the creep resistance behavior was opposite at relatively low load levels. This difference in creep resistance was explained based on the difference in the creep deformation and/or fracture mechanism.

Idioma originalInglés
Título de la publicación alojadaTMS 2010 - 139th Annual Meeting and Exhibition - Supplemental Proceedings
Páginas729-736
Número de páginas8
EstadoPublicada - 2010
Publicado de forma externa
EventoTMS 2010 - 139th Annual Meeting and Exhibition - Seattle, WA, Estados Unidos
Duración: 14 feb. 201018 feb. 2010

Serie de la publicación

NombreTMS Annual Meeting
Volumen3

Conferencia

ConferenciaTMS 2010 - 139th Annual Meeting and Exhibition
País/TerritorioEstados Unidos
CiudadSeattle, WA
Período14/02/1018/02/10

Huella

Profundice en los temas de investigación de 'Small punch creep test of service-exposed SUS 316 HTB superheater tubes of fossil boilers'. En conjunto forman una huella única.

Citar esto