In this work we report the characterization and results of hydrothermal treatment tests performed on MCM-41 and Ti-MCM-41 materials at two temperatures, 450 and 550°C. Based on BET analyses and XRD measurements, results showed a decrease in specific surface area, pore volume and pore size for both materials after the hydrothermal treatments. The Ti-MCM-41 material was more stable than the MCM-41. The specific surface area reduction for the hydrothermally treated Ti-MCM-41 samples at 450 and 550°C was 16% and 29%, respectively. Similarly, there was a reduction of the interplanar spacing of 30% and 33%, respectively, observed as a displacement of the main diffraction peak towards larger diffraction angles. We also report the conversion and selectivity of these materials in the HDS reaction of DBT. A higher conversion was obtained with the Ti-MCM-41 supported catalyst.

Idioma originalInglés
Páginas (desde-hasta)115-121
Número de páginas7
PublicaciónCatalysis Today
Volumen98
N.º1-2 SPEC. ISS.
DOI
EstadoPublicada - 24 nov. 2004
Publicado de forma externa

Huella

Profundice en los temas de investigación de 'Characterization of hydrothermally treated MCM-41 and Ti-MCM-41 molecular sieves'. En conjunto forman una huella única.

Citar esto