Abstract

Er3+-Tm3+ co-doped tellurite photonic crystal fiber was fabricated via a stack-and-draw procedure and without using extrusion in any stage. The final fiber presents a 187 nm bandwidth of amplified spontaneous emission (ASE) intensity around 1550nm when pumped with 790nm. In this manuscript a soft-glass tube fabrication technique, using the centrifugation method, is also shown.

Original languageEnglish
Title of host publicationProceedings of SPIE - The International Society for Optical Engineering
DOIs
StatePublished - 2006
Externally publishedYes
EventOptical Components and Materials III - San Jose, CA, United States
Duration: 23 Jan 200625 Jan 2006

Publication series

NameProceedings of SPIE - The International Society for Optical Engineering
Volume6116
ISSN (Print)0277-786X

Conference

ConferenceOptical Components and Materials III
Country/TerritoryUnited States
CitySan Jose, CA
Period23/01/0625/01/06

Keywords

  • Centrifugation
  • Erbium-Thulium fiber
  • Optical amplifier
  • Tellurite Photonic Crystal Fiber

Fingerprint

Dive into the research topics of 'Tellurite photonic crystal fiber with Er3+-Tm3+ for broadband optical amplifier in 1550nm'. Together they form a unique fingerprint.

Cite this