This work presents a study on the behavior of stress corrosion cracking (SCC) phenomenon in pipeline steels for sour service in near-neutral media. SCC tests under static stressing conditions were performed in planar steel samples using a Cortest proof-ring coupled with a fabricated cell containing near-neutral pH solution as a corrosive medium, which simulates the soil conditions, to observe the cracking initiation stage. Characterizations of the steel samples using surface techniques such as SEM, EDS, and Raman spectroscopy show that the presence of nonmetallic inclusions takes place as pitting sites (to form corrosion pits), which constitute the most susceptible sites for SCC crack initiation. SEM images taken on the steel sample surfaces exhibit both SCC transgranular and intergranular crack types in near-neutral media. Although the obtained results are interesting, further study is necessary to evaluate and confirm the role of inclusions in SCC initiation mechanisms.

Original languageEnglish
Title of host publicationAdvances in Engineering Research and Application - Proceedings of the International Conference on Engineering Research and Applications, ICERA 2021
EditorsDuy Cuong Nguyen, Ngoc Pi Vu, Banh Tien Long, Horst Puta, Kai-Uwe Sattler
PublisherSpringer Science and Business Media Deutschland GmbH
Pages855-861
Number of pages7
ISBN (Print)9783030925734
DOIs
StatePublished - 2022
Externally publishedYes
EventInternational Conference on Engineering Research and Applications, ICERA 2021 - Thai Nguyen, Viet Nam
Duration: 1 Dec 20212 Dec 2021

Publication series

NameLecture Notes in Networks and Systems
Volume366 LNNS
ISSN (Print)2367-3370
ISSN (Electronic)2367-3389

Conference

ConferenceInternational Conference on Engineering Research and Applications, ICERA 2021
Country/TerritoryViet Nam
CityThai Nguyen
Period1/12/212/12/21

Keywords

  • Initiation stage
  • Pipeline steel
  • Stress corrosion cracking

Fingerprint

Dive into the research topics of 'Stress Corrosion Cracking Behavior in API 5L Steels for Sour Service'. Together they form a unique fingerprint.

Cite this