Oxidative dehydrogenation of n-octane over Mg-containing SBA-15 material

Elienaí Gaxiola, F. F. Castillón, José A. Hernández, B. Acosta, J. N. Díaz de León, S. Fuentes, T. A. Zepeda

    Research output: Contribution to journalArticlepeer-review

    3 Scopus citations

    Abstract

    In this study, it is proposed the incorporation of MgO into of SBA-15 via the direct synthesis different atomic ratios of Si/Mg (20, 40 and 80). Although the incorporation of Mg did not affect the mesoporous character of SBA-based materials, it was found dramatic changes in the SBA-15 characteristic honeycomb structure even after the incorporation of small amount of Mg. The creation of more basic sites in SBA-15, because of the addition of Mg, improved ODH conversion of n-octane with respect to SBA-15, used as reference. Sample with a Si/Mg molar ratio of 20 showed the best catalytic performance in the oxidative dehydrogenation of n-octane, while the sample with a Si/Mg molar ratio of 40 achieve the highest productions of olefins.

    Original languageEnglish
    Pages (from-to)247-253
    Number of pages7
    JournalMaterials Research Innovations
    Volume22
    Issue number5
    DOIs
    StatePublished - 29 Jul 2018

    Keywords

    • Mesoporous silica SBA-15
    • Mg-SBA-15
    • oxidative dehydrogenation of n-octane