N2 - This chapter describes the adequate methodology for the examination of fractured components, with emphasis being given to the specific features of fractured components that have to be recorded for further analysis. The correct procedures for the handling, cutting, cleaning and preservation of fractures are described in detail. Recommendations for taking good photographs of fractured surfaces are given, including a description of the fundamentals of digital photography. The chapter ends with a description of the elaboration of fracture replicas.
AB - This chapter describes the adequate methodology for the examination of fractured components, with emphasis being given to the specific features of fractured components that have to be recorded for further analysis. The correct procedures for the handling, cutting, cleaning and preservation of fractures are described in detail. Recommendations for taking good photographs of fractured surfaces are given, including a description of the fundamentals of digital photography. The chapter ends with a description of the elaboration of fracture replicas.
UR - http://www.scopus.com/inward/record.url?scp=85085303789&partnerID=8YFLogxK
U2 - 10.1007/978-3-319-76651-5_1
DO - 10.1007/978-3-319-76651-5_1
M3 - Capítulo
AN - SCOPUS:85085303789
T3 - Structural Integrity
SP - 1
EP - 20
BT - Structural Integrity
PB - Springer
ER -