Formation of Co-Sn alloys by mechanical alloying

V. M. Lopez Hirata, U. Juarez Martinez, J. G. Cabanas-Moreno

Producción científica: Contribución a una revistaArtículo de la conferenciarevisión exhaustiva

2 Citas (Scopus)

Resumen

Co-10, 20, 30, 40, 50 and 60 at. % Sn powder mixtures were milled for 1080 ks in a conventional ball mill. The as-milled powders were analyzed by XRD, TEM, SEM and DSC. XRD patterns of as-milled Co-10 and 20 at. % Sn powders showed the presence of an amorphous-like phase, while those of other compositions presented crystalline phases. Crystallization temperature and activation energy of crystallization of amorphous Co-10 and 20 at. Sn mechanical alloys showed a good agreement with values reported by other authors. TEM observation of as-milled Co-10 and 20 at. % Sn powders revealed a crystalline phase of nanometer-order size dispersed in the amorphous phase.

Idioma originalInglés
Páginas (desde-hasta)261-266
Número de páginas6
PublicaciónMaterials Science Forum
Volumen179-181
DOI
EstadoPublicada - 1995
EventoProceedings of the International Symposium on Metastable, Mechanically Alloyed and Nanocrystalline Materials - Grenoble, Fr
Duración: 27 jun. 19941 jul. 1994