N2 - Chemical and mineralogical characterization of a sulphide ore from the mining district of Zimapan, Hidalgo, Mexico, was performed in order to obtain accurate information on the composition of the ore to optimize the subsequent flotation process. A combination of techniques was used: Scanning Electron Microscopy (SEM) with Energy Dispersive Spectrometer (EDS), X-ray diffractometry (XRD), Inductively Coupled Plasma (ICP) and Fourier transform infrared spectroscopy (FTIR). The SEM mapping confirmed the presence of the elements: Ca, Si, Fe, K, S, Al, Zn, Mg and Mn. The XRD analysis suggests that the ore matrix is calcite; additional species found were wollastonite, johannsenite, and pyrite, among other impurities. The FTIR analysis performed for the aqua regia insoluble showed the presence of calcium oxide, copper oxide and silicon oxide. The results for the ICP analysis were:13.31% S, 2.55% Fe, 0.46% Zn, 0.03% Cu, 0.06% Pb, 0.07% Mn, 0.09% As, 0.01% Sb and 0.08 grton-1 Ag.
AB - Chemical and mineralogical characterization of a sulphide ore from the mining district of Zimapan, Hidalgo, Mexico, was performed in order to obtain accurate information on the composition of the ore to optimize the subsequent flotation process. A combination of techniques was used: Scanning Electron Microscopy (SEM) with Energy Dispersive Spectrometer (EDS), X-ray diffractometry (XRD), Inductively Coupled Plasma (ICP) and Fourier transform infrared spectroscopy (FTIR). The SEM mapping confirmed the presence of the elements: Ca, Si, Fe, K, S, Al, Zn, Mg and Mn. The XRD analysis suggests that the ore matrix is calcite; additional species found were wollastonite, johannsenite, and pyrite, among other impurities. The FTIR analysis performed for the aqua regia insoluble showed the presence of calcium oxide, copper oxide and silicon oxide. The results for the ICP analysis were:13.31% S, 2.55% Fe, 0.46% Zn, 0.03% Cu, 0.06% Pb, 0.07% Mn, 0.09% As, 0.01% Sb and 0.08 grton-1 Ag.
KW - Characterization
KW - Flotation
KW - Sulphide ore
KW - Zimapan
UR - http://www.scopus.com/inward/record.url?scp=85042349293&partnerID=8YFLogxK
U2 - 10.1007/978-3-319-51382-9_67
DO - 10.1007/978-3-319-51382-9_67
M3 - Contribución a la conferencia
SN - 9783319513812
T3 - Minerals, Metals and Materials Series
SP - 607
EP - 615
BT - Characterization of Minerals, Metals, and Materials 2017
A2 - Li, Jian
A2 - Monteiro, Sergio Neves
A2 - Escobedo-Diaz, Juan P.
A2 - Kim, Jeongguk
A2 - Goswami, Ramasis
A2 - Hwang, Jiann-Yang
A2 - Kalay, Yunus Eren
A2 - Li, Bowen
A2 - Zhang, Mingming
A2 - Ikhmayies, Shadia
A2 - Carpenter, John S.
A2 - Peng, Zhiwei
A2 - Firrao, Donato
A2 - Bai, Chenguang
PB - Springer International Publishing
T2 - International Symposium on Characterization of Minerals, Metals, and Materials, 2017
Y2 - 26 February 2017 through 2 March 2017
ER -